Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 8.439 MPa | 1224 psi | ASTM D882 |
Dow ELITE™ 5500G Enhanced Polyethylene Resin ™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te.. |