Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 7.17 MPa | 1040 psi | ASTM D882 |
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP) AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In.. |