Film Tensile Strength at Yield, TD 37.5 MPa
5440 psi
ASTM D882
Reliance Industries Relene E52009 Polyethylene
Relene E52009 is a High Density Polyethylene grade with low gel content, excellent orientation characteristics and negligible water carry-over. This grade is recommended for making raffia tapes and..