Film Tensile Strength at Yield, TD 36.0 MPa
5220 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PPE 1461  (discontinued **)
PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
Film Tensile Strength at Yield, TD 36.0 MPa

@Temperature 23.0 °C
5220 psi

@Temperature 73.4 °F
ASTM D638
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet
Maplon Catalog No. L050-C001K0101 is an extremely opaque white sheet. Sheet surface is smoothly embossed with similar finish on both sides..Main advantages: High opacity, High rigidity high thermal ..