Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 39.2 MPa
5690 psi
ASTM D828
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..