Polymer Property : Film Tensile Strength at Yield, TD = 3735 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 25.75 MPa
3735 psi
ASTM D882
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe..