Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 14.7 - 29.6 MPa
2130 - 4300 psi
Average value: 20.1 MPa Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..