Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 16.7 MPa
2420 psi
ASTM D882
Bapolene® 122F Polyethylene, Film Grade
Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. ..