Polymer Property : Film Tensile Strength at Yield, TD = 11.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 11.8 MPa
1710 psi
at 2% offset; ASTM D882
ExxonMobil LD 071.MU Blown Film Resin  (discontinued **)
LD 071 series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, toughness, burn-through re..
Film Tensile Strength at Yield, TD 11.8 MPa
1710 psi
ASTM D882
ExxonMobil LD 071.LQ Blown Film Resin
L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou..
Film Tensile Strength at Yield, TD 11.8 MPa
1710 psi
ASTM D882
ExxonMobil LD 071.LR Blown Film Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Film Tensile Strength at Yield, TD 11.8 MPa
1710 psi
ASTM D882
Dow DOWLEX™ 2021D Linear Low Density Polyethylene
Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow