Polymer Property : Izod Impact Resistance = 5.71 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
cond; ISO 180/1A
DSM Stanyl® TE200F8 PA46-GF40
40% Glass Reinforced, Heat Stabilized, for E&E applications
Izod Impact Resistance 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
dry; ISO 180/1A
DSM Stanyl® TE200F8 PA46-GF40
40% Glass Reinforced, Heat Stabilized, for E&E applications
Izod Impact Resistance 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
cond; ISO 180/1A
DSM Stanyl® TS250F8 PA46-GF40 FR
40% Glass Reinforced, Flame Retardant, Heat Stabilized
Izod Impact Resistance 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
DSM Stanyl® TS250F8 PA46-GF40 FR
40% Glass Reinforced, Flame Retardant, Heat Stabilized
Izod Impact Resistance 1.20 J/cm²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
dry; ISO 180/1A
DSM Stanyl® TS250F8 PA46-GF40 FR
40% Glass Reinforced, Flame Retardant, Heat Stabilized
Izod Impact Resistance 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 180/1A
DSM Stanyl® TW241B3 PA46-CF15
15% Carbon Reinforced, Heat Stabilized, Lubricated
Izod Impact Resistance 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 180/1A
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15
15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
Izod Impact Resistance 1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
DSM Stanyl® TS200F6 PA46-GF30
30% Glass Reinforced