Polymer Property : Izod Impact Resistance = 11.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 180/1A
DSM Stanyl® OCD2100 BK27021 PA46-GF40
40% Glass Reinforced, Heat Stabilized