Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 610 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
610 g/in @Pressure 40.0 psi, Temperature 266 °F |
Acrylic, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 32MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin.. |
|||
Seal Strength | 610 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
610 g/in @Pressure 40.0 psi, Temperature 266 °F |
Acrylic, 0.2 sec; ExxonMobil Method |
ExxonMobil Bicor™ 42MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi.. |
|||
Seal Strength | 610 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
610 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Bruger, 0.5 sec; ExxonMobl Method |
ExxonMobil Bicor™ 52MBR666 OPP Film Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo.. |