Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
0.5 sec, LPS; ExxonMobl Method
ExxonMobil Bicor™ 21MB621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both sides. The static resistant feature of this film prevents the attraction of dust, an..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
LSP, 0.5 sec; ExxonMobil Method
ExxonMobil Bicor™ 26MB600 OPP Film
Product Description: Biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, Asia..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
LPS, 0.5 sec; ExxonMobil Method
ExxonMobil Bicor™ 32MB600 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
LPS, 0.5 sec; ExxonMobl Method
ExxonMobil Bicor™ 52MBR666 OPP Film
Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo..