Mechanical Properties Metric English Comments
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3100 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 3158 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® ET3117 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® FU4007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Puncture Resistance 6500 N

@Temperature -30.0 °C
1460 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..