Puncture Resistance 6200 N

@Temperature -30.0 °C
1390 lb (f)

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..