Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Wear | 0.220 mm @Temperature 75.0 °C, Time 3600 sec |
0.00866 in @Temperature 167 °F, Time 1.00 hour |
1200 rpm, 10 kg, scar diameter; ASTM D2266, DIN 51 350 |
Chesterton 610 Synthetic Lubricating Fluid Description: Chesterton® 610 Synthetic Lubrication Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from -25°C (-15°F) for those over 27.. |