Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.94 g/micron @Thickness 0.0254 mm |
100 g/mil @Thickness 0.00100 in |
High Stalk Extrusion - 6:1 FLH/D ratio and 4:1 BUR; ASTM D1709A |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |