Dart Drop <= 1.97 g/micron

@Thickness 0.0254 mm
<= 50.0 g/mil

@Thickness 0.00100 in
2.5 BUR; ASTM D1709A
Total HL 428 HDPE Film Grade
Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro..