Polymer Property : Shear Modulus = 99.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.683 GPa
99.1 ksi
Calculated
Metton LMR M1534 Liquid Molding Resin
Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce ..