Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 64.9 GPa | 9410 ksi | Calculated |
Ceradyne Ceralloy® 398J Yttrium Oxide Ceralloy® 398J Hot Pressed Yttrium Oxide is a high purity hot-pressed ceramic exhibiting excellent corrosion and erosion resistance. Products produced from Hot Pressed Yttrium Oxide are for semicon.. |