Mechanical Properties Metric English Comments
Shear Modulus 60.0 GPa
8700 ksi
Calculated
CoorsTek Mullite, S2
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..