Polymer Property : Shear Modulus = 84.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.580 GPa
84.1 ksi
DIN 53457
Global PP-2300-LC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme..
Shear Modulus 0.580 GPa
84.1 ksi
DIN 53457
Global PP-3342-M Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-housewares, cookwareInformation provided by Global Polymers Corporation.