Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 80.0 GPa @Temperature 20.0 °C |
11600 ksi @Temperature 68.0 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Shear Modulus | 80.0 GPa | 11600 ksi | cold-rolled, heat treated sheet |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re.. |
|||
Shear Modulus | 80.0 GPa | 11600 ksi | cold-rolled, heat treated sheet |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (.. |
|||
Shear Modulus | 80.0 GPa | 11600 ksi | |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Shear Modulus | 80.0 GPa | 11600 ksi | Calculated |
M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |
|||
Shear Modulus | 80.0 GPa | 11600 ksi | |
CeramTec 848 Zirconia, ZrO2•MgO Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i.. |