Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 49.1 GPa | 7120 ksi | calculated |
Materion ToughMet® T3 CA ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Shear Modulus | 49.1 GPa | 7120 ksi | calculated |
Materion ToughMet® T3 CX105 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Shear Modulus | 49.1 GPa | 7120 ksi | calculated |
Materion ToughMet® T3 CX90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Shear Modulus | 49.1 GPa | 7120 ksi | calculated |
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |