Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 47.0 GPa | 6820 ksi | calculated |
Schott N-LAK33A Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 47.0 GPa | 6820 ksi | |
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses .. |