Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 6.34 GPa | 920 ksi | Calculated |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |