Polymer Property : Shear Modulus = 5510 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 38.0 GPa
5510 ksi
Calculated
Schott Dark ROBAX® Glass Ceramic
Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolle..
Shear Modulus 38.0 GPa
5510 ksi
calculated
Schott N-SF57 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 38.0 GPa
5510 ksi
calculated
Schott N-SF66 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 38.0 GPa
5510 ksi
calculated
Schott N-LAF7 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 38.0 GPa
5510 ksi
calculated
Schott N-SF57HT Glass
Information Provided by SCHOTT North America, Inc.