Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.67 - 6.10 GPa | 822 - 885 ksi | Calculated |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |