Mechanical Properties Metric English Comments
Shear Modulus 5.58 GPa
809 ksi
Calculated
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
Shear Modulus 5.58 GPa
809 ksi
Calculated
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..