Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.14 GPa | 746 ksi | Calculated |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |