Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.42 - 5.11 GPa | 496 - 741 ksi | Calculated |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Shear Modulus | 3.42 GPa | 496 ksi | Calculated |
Plenco 4304 Phenolic, Nodular, Transfer Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |