Polymer Property : Shear Modulus = 49.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 49.6 GPa
7200 ksi
Cadi 1815 Copper Alloy
Zirconium addition to chromium copper improves creep resistance at high operating temperatures and reportedly reduces sticking of electrodes to the work during spot welding of galvanized materials. ..
Shear Modulus 49.6 GPa
7200 ksi
Cadi 182 Copper Alloy
Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold ..