Polymer Property : Shear Modulus = 47.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 47.9 GPa
6950 ksi
calculated
Materion ToughMet® T3 AT110 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Shear Modulus 47.9 GPa
6950 ksi
calculated
Materion ToughMet® T3 AT120 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Shear Modulus 47.9 GPa
6950 ksi
calculated
Materion ToughMet® T3 AT120 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Shear Modulus 47.9 GPa
6950 ksi
calculated
Materion ToughMet® T3 AT90 (OD≥4")
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Shear Modulus 47.9 GPa
6950 ksi
calculated
Materion ToughMet® T3 AT110 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin..
Shear Modulus 47.9 GPa
6950 ksi
calculated
Materion ToughMet® T3 AT90 (OD
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin..