Shear Modulus 46.0 GPa
6670 ksi
calculated
Schott P-LASF47 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Shear Modulus 46.0 GPa
6670 ksi
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged
High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i..