Polymer Property : Shear Modulus = 4500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 31.0 GPa
4500 ksi
Momentive Performance Materials Type 214 Fused Quartz Tubing
Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo..
Shear Modulus 31.0 GPa
4500 ksi
calculated
Schott LAFN7 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 31.0 GPa
4500 ksi
calculated
Schott LITHOSIL-Q Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 31.0 GPa
4500 ksi
calculated
Schott N-BAK4 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 31.0 GPa
4500 ksi
calculated
Schott N-BALF4 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 31.0 GPa
4500 ksi
calculated
Schott N-SK2 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain HS Grade Optical Fused Quartz
HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, ..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz
Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz
Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz
Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz
Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 ..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Vitreosil® 055 Optical Fused Quartz
Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz
Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt..
Shear Modulus 31.0 GPa
4500 ksi
calculated
Schott N-KZFS4 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz
Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra..
Shear Modulus 31.0 GPa
4500 ksi
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz
Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i..