Mechanical Properties Metric English Comments
Shear Modulus 42.7 - 44.8 GPa
6200 - 6500 ksi
ATI Wah Chang TI-3Al-2.5V
Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an..