Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 30.0 GPa | 4350 ksi | calculated |
Piezo Kinetics 406 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars. PKI 406 is suitabl.. |
|||
Shear Modulus | 30.0 GPa | 4350 ksi | calculated |
Schott LITHOTEC-CAF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 30.0 GPa | 4350 ksi | calculated |
Schott N-BK10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 30.0 GPa | 4350 ksi | calculated |
Schott N-PSK53A Glass Information Provided by SCHOTT North America, Inc. |