Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 4.62 GPa
670 ksi
Calculated
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP
SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord..