Polymer Property : Shear Modulus = 4.50 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0310 GPa
4.50 ksi
Plate Shear, W Direction, typical value
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.0 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..
Shear Modulus 0.0310 GPa
4.50 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Modulus 0.0310 GPa
4.50 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10 - 1/2 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..