Mechanical Properties Metric English Comments
Shear Modulus 4.47 GPa
648 ksi
Calculated
Plenco 7552 Phenolic, Nodular, Injection Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..