Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-BAF51 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-SF1 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-SF15 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-SF4 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott P-SF67 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-LAF2 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-LAK21 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-LAK22 Glass
Information Provided by SCHOTT North America, Inc.
Shear Modulus 36.0 GPa
5220 ksi
Calculated
Advanced Ceramics ZEMAT® ACL 2090 - Zero Expansion Glass-Ceramic
“Zero Expansion” glass-ceramic is a transparent material now in production for applications requiring ultra-low thermal expansion. The primary crystal phase is a s-eucryptite (Li2OAl2O32SiO2) soli..
Shear Modulus 36.0 GPa
5220 ksi
calculated
Schott N-KZFS5 Glass
Information Provided by SCHOTT North America, Inc.