Polymer Property : Shear Modulus = 33.7 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 33.7 GPa
4890 ksi
Calculated
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass
Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube ..