Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 32.0 GPa | 4640 ksi | calculated |
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 32.0 GPa | 4640 ksi | calculated |
Schott N-SK11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 32.0 GPa | 4640 ksi | |
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures... |