Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 30.4 GPa | 4410 ksi | Calculated |
Schott DUROBAX® clear Neutral Glass Tubing Neutral glass tubing, chemically highly resistant Syringes, cartridges, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is.. |