Mechanical Properties Metric English Comments
Shear Modulus 0.207 GPa
30.0 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP - 3/16 - 7.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Modulus 0.207 GPa
30.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Modulus 0.207 GPa
30.0 ksi
Plate Shear, L Direction, typ, preliminary value obtained at .500 inch thickness
Hexcel® HexWeb® HRH-327 - 1/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Modulus 0.207 GPa

@Strain <=100 %
30.0 ksi

@Strain <=100 %
ASTM D1002
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Shear Modulus 0.207 GPa
30.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 3/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..