Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0230 GPa | 3.34 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Shear Modulus | 0.0230 GPa | 3.34 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |