Polymer Property : Shear Modulus = 3.23 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 3.23 GPa
468 ksi
Calculated
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, ..