Mechanical Properties Metric English Comments
Shear Modulus 3.20 - 3.84 GPa
464 - 557 ksi
Average value: 3.66 GPa Grade Count:4
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Shear Modulus 3.20 GPa
464 ksi
Calculated
Plenco 3509 Phenolic, Granular, Injection Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..