Polymer Property : Shear Modulus = 290 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 2.00 - 2.40 GPa

@Temperature 130 - 130 °C
290 - 348 ksi

@Temperature 266 - 266 °F
Average value: 2.20 GPa Grade Count:2
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Shear Modulus 2.00 GPa

@Temperature 130 °C
290 ksi

@Temperature 266 °F
In-Plane, Wet; EN6031
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber
Information provided by HexCel