Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 29.6 GPa | 4300 ksi | |
Potters Industries Spheriglass® 1922 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Shear Modulus | 29.6 GPa | 4300 ksi | |
Potters Industries Spheriglass® 2024 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Shear Modulus | 29.6 GPa | 4300 ksi | |
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Shear Modulus | 29.6 GPa | 4300 ksi | |
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Shear Modulus | 29.6 GPa | 4300 ksi | |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Shear Modulus | 29.6 GPa | 4300 ksi | |
Potters Industries Spheriglass® 5000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Shear Modulus | 29.6 GPa | 4290 ksi | |
Corning Large Cover Gorilla® Glass Touch Screen Glass Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C.. |
|||
Shear Modulus | 29.6 GPa | 4290 ksi | |
Mateck Window Grade Zinc Selenide, ZnSe Optical Crystals |